摘要: |
用DSC和TG DTG等热分析手段研究了过冷态和结晶态的键合剂 1,1’ (1,3 苯二羰基 )双 2 甲基氮丙啶(HX 75 2 )的热行为 ,在 - 80℃~ 10 0℃范围内 ,除了过冷态在 - 37.6℃的玻璃化转变和结晶态在 36 .8℃~ 42 .9℃的熔融外 ,没有任何其它物理化学变化。亚稳态的过冷液体比结晶态有较大的分解热。HX 75 2有复杂的分解过程 ,第一步分解失重虽小 ,但放热量很大 ,说明分子结构发生重大变化。 |
关键词: 复合推进剂 键合剂 热分解 热分析 |
DOI: |
分类号:V5123 |
基金项目: |
|
Thermal behavior of bonding agent 1,1′-(1,3-phenylenedlcarbonyl) bis-2-methyl-aziridine |
WANG Yi-ying, QIU Gang
|
Xi’an Hongda New Chemical Materials Company, Xi’an 710065,China
|
Abstract: |
The thermal behavior of either bulk-crystallized solid or super-cooled liquid of bonding agent 1,1’-(1,3-phenylenedlcarbonyl) bis-2-methyl-aziridine(HX-752)was investigated by DSC and TG-DTG. No physics and chemistry changes were found in the range of -80 ℃~100 ℃ except that the super-cooled liquid transform to the glass at -37.6 ℃ and the crystallized solid melt at 36 8 ℃~42 9 ℃.The decomposition heat for metastable super-cooled liquid is greater than that of crystallized solid. It is shown that thermal decomposition process of HX-752 is complicated although the mass-loss is relatively small, the release heat is great at the first step. It indicates that significant changes in the molecular constitution on the decomposition is happened. |
Key words: Composite propellant Bonding agent Thermal decomposition Thermal analysis |